Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.890 - 1.21 g/cc
0.0322 - 0.0437 lb/in³
Average value: 1.06 g/cc Grade Count:130
Water Absorption 0.0500 - 1.00 %
0.0500 - 1.00 %
Average value: 0.598 % Grade Count:21
Moisture Absorption at Equilibrium 0.200 - 0.250 %
0.200 - 0.250 %
Average value: 0.208 % Grade Count:13
Viscosity 225000 - 255000 cP

@Temperature 260 - 260 °C
225000 - 255000 cP

@Temperature 500 - 500 °F
Average value: 245000 cP Grade Count:3
Maximum Moisture Content 0.0100 - 0.0200
0.0100 - 0.0200
Average value: 0.0104 Grade Count:27
Linear Mold Shrinkage 0.00200 - 0.00800 cm/cm
0.00200 - 0.00800 in/in
Average value: 0.00552 cm/cm Grade Count:106
Linear Mold Shrinkage, Transverse 0.00200 - 0.00640 cm/cm
0.00200 - 0.00640 in/in
Average value: 0.00570 cm/cm Grade Count:11
Melt Flow 0.200 - 26.0 g/10 min
0.200 - 26.0 g/10 min
Average value: 5.91 g/10 min Grade Count:136
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100 - 116
100 - 116
Average value: 109 Grade Count:89
Ball Indentation Hardness 95.0 - 115 MPa
13800 - 16700 psi
Average value: 104 MPa Grade Count:13
Tensile Strength, Ultimate 19.6 - 49.0 MPa
2840 - 7110 psi
Average value: 39.8 MPa Grade Count:29
Tensile Strength, Yield 33.0 - 108 MPa
4790 - 15600 psi
Average value: 46.4 MPa Grade Count:125
Elongation at Break 2.50 - 70.0 %
2.50 - 70.0 %
Average value: 23.7 % Grade Count:78
Elongation at Yield 2.00 - 6.00 %
2.00 - 6.00 %
Average value: 3.19 % Grade Count:44
Modulus of Elasticity 1.70 - 2.70 GPa
247 - 392 ksi
Average value: 2.27 GPa Grade Count:50
Flexural Yield Strength 45.6 - 142 MPa
6610 - 20600 psi
Average value: 73.4 MPa Grade Count:87
Flexural Modulus 1.73 - 6.86 GPa
250 - 996 ksi
Average value: 2.41 GPa Grade Count:106
Izod Impact, Notched 0.392 - 4.00 J/cm
0.735 - 7.49 ft-lb/in
Average value: 1.77 J/cm Grade Count:104
0.370 - 1.60 J/cm

@Temperature -40.0 - 0.000 °C
0.693 - 3.00 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.826 J/cm Grade Count:10
0.588399 - 0.686465 J/cm

@Temperature -30.0 - -30.0 °C
1.10231 - 1.28603 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.826 J/cm Grade Count:1
0.588399 - 0.686465 J/cm

@Thickness 3.17 - 6.35 mm
1.10231 - 1.28603 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 0.826 J/cm Grade Count:1
Izod Impact, Unnotched 0.392266 - 1.27486 J/cm

@Temperature -30.0 - -30.0 °C
0.734875 - 2.38834 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.824 J/cm Grade Count:26
0.392266 - 1.27486 J/cm

@Thickness 3.20 - 6.40 mm
0.734875 - 2.38834 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 0.824 J/cm Grade Count:26
Izod Impact, Notched (ISO) 10.0 - 32.0 kJ/m²
4.76 - 15.2 ft-lb/in²
Average value: 17.7 kJ/m² Grade Count:15
4.00 - 12.0 kJ/m²

@Temperature -30.0 - -30.0 °C
1.90 - 5.71 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.83 kJ/m² Grade Count:10
Charpy Impact Unnotched 6.00 J/cm² - NB
28.6 ft-lb/in² - NB
Average value: 12.5 J/cm² Grade Count:35
5.00 - 18.0 J/cm²

@Temperature -30.0 - -30.0 °C
23.8 - 85.7 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 10.5 J/cm² Grade Count:22
Charpy Impact, Notched 0.600 - 3.20 J/cm²
2.86 - 15.2 ft-lb/in²
Average value: 1.58 J/cm² Grade Count:39
0.300 - 1.30 J/cm²

@Temperature -30.0 - -20.0 °C
1.43 - 6.19 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.774 J/cm² Grade Count:27
Gardner Impact 2.71 - 22.6 J
2.00 - 16.7 ft-lb
Average value: 12.6 J Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 0.700 - 102 µm/m-°C
0.389 - 56.7 µin/in-°F
Average value: 78.3 µm/m-°C Grade Count:41
Thermal Conductivity 0.128 - 0.200 W/m-K
0.888 - 1.39 BTU-in/hr-ft²-°F
Average value: 0.161 W/m-K Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 91.0 - 122 °C
196 - 252 °F
Average value: 105 °C Grade Count:84
Deflection Temperature at 1.8 MPa (264 psi) 76.7 - 130 °C
170 - 266 °F
Average value: 98.1 °C Grade Count:122
Vicat Softening Point 97.0 - 165 °C
207 - 329 °F
Average value: 111 °C Grade Count:111
Glass Transition Temp, Tg 108 - 127 °C
226 - 261 °F
Average value: 116 °C Grade Count:9
UL RTI, Electrical 50.0 - 85.0 °C
122 - 185 °F
Average value: 62.0 °C Grade Count:20
UL RTI, Mechanical with Impact 50.0 - 85.0 °C
122 - 185 °F
Average value: 62.0 °C Grade Count:20
UL RTI, Mechanical without Impact 50.0 - 85.0 °C
122 - 185 °F
Average value: 62.0 °C Grade Count:20
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:76
Glow Wire Test 650 - 750 °C
1200 - 1380 °F
Average value: 664 °C Grade Count:6
Optical Properties Metric English Comments
Gloss 30.0 - 98.0 %
30.0 - 98.0 %
Average value: 65.7 % Grade Count:15
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 - 1.00e+16 ohm-cm
1.00e+14 - 1.00e+16 ohm-cm
Average value: 1.46e+15 ohm-cm Grade Count:33
Surface Resistance 1.00e+14 - 1.00e+16 ohm
1.00e+14 - 1.00e+16 ohm
Average value: 1.00e+15 ohm Grade Count:19
Dielectric Constant 2.70 - 3.20
2.70 - 3.20
Average value: 3.00 Grade Count:19
Dielectric Strength 18.0 - 41.0 kV/mm
457 - 1040 kV/in
Average value: 32.1 kV/mm Grade Count:36
Dissipation Factor 0.00400 - 0.0130
0.00400 - 0.0130
Average value: 0.00747 Grade Count:19
Arc Resistance 60.0 - 120 sec
60.0 - 120 sec
Average value: 90.0 sec Grade Count:14
Comparative Tracking Index 250 - 600 V
250 - 600 V
Average value: 593 V Grade Count:37
Hot Wire Ignition, HWI 7.00 - 60.0 sec
7.00 - 60.0 sec
Average value: 20.7 sec Grade Count:14
High Amp Arc Ignition, HAI 30.0 - 120 arcs
30.0 - 120 arcs
Average value: 111 arcs Grade Count:14
High Voltage Arc-Tracking Rate, HVTR 10.0 - 150 mm/min
0.394 - 5.91 in/min
Average value: 38.6 mm/min Grade Count:14