Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.523 - 1.12 J/cm | 0.980 - 2.10 ft-lb/in | Average value: 0.733 J/cm Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.600 - 1.12 J/cm @Temperature -30.0 - -30.0 °C |
1.12 - 2.10 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.864 J/cm Grade Count:9 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Notched | 0.534 - 1.12 J/cm | 1.00 - 2.10 ft-lb/in | Average value: 0.798 J/cm Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Izod Impact, Notched | 0.883 - 1.12 J/cm | 1.65 - 2.10 ft-lb/in | Average value: 0.970 J/cm Grade Count:3 |
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
Izod Impact, Notched | 0.320 - 1.12 J/cm | 0.600 - 2.10 ft-lb/in | Average value: 0.767 J/cm Grade Count:8 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Izod Impact, Notched | 0.530 - 1.12 J/cm | 0.993 - 2.10 ft-lb/in | Average value: 0.793 J/cm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Izod Impact, Notched | 1.01 - 1.12 J/cm | 1.90 - 2.10 ft-lb/in | Average value: 1.07 J/cm Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% .. |