Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.39 J/cm @Temperature 23.0 °C |
2.60 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature 23.0 °C |
2.60 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P251-00 Polypropylene Copolymer, Natural Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature 23.0 °C |
2.60 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P256-00 Polypropylene Copolymer, Natural Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature -30.0 °C |
2.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS6 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature -30.0 °C |
2.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS6 PC (Asia Pacific) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature 23.0 °C |
2.60 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature -40.0 °C |
2.60 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman EASTALLOY Polymer DA105, Natural Alloy
(discontinued **) General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman ma.. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature -30.0 °C |
2.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature -30.0 °C |
2.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature -30.0 °C |
2.60 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
Covestro Petlon® PC/PET 36A 620UV Yellow Semi-Crystalline PET, 10% Glass Fiber
(discontinued **) Characteristics: Good Thermal and Dimensional Stability, Good Chemical ResistanceApplications: Automotive Panels, Electronic Housings, Pump HousingsProcessing: Injection Molding (Melt Temperature: 5.. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
Global GPP-2500 Polypropylene Impact Copolymer, Nucleated Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DX09407H PC LNP* LUBRICOMP* DX09407H is a compound based on High Heat Polycarbonate containing proprietary fillers. Added features of this grade are: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 1.39 J/cm @Thickness 3.17 mm |
2.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF44 HS X 44% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 44% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized TPCI# 95.. |
|||
Izod Impact, Notched | 1.39 J/cm @Thickness 3.17 mm |
2.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF43 L BK001 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackTPCI# 7176101Information provi.. |
|||
Izod Impact, Notched | 1.39 J/cm @Thickness 3.17 mm |
2.60 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plaslube® J-3/30/TF/13/SI/2 Nylon 6, 30% GFR, 13% PTFE, 2% Silicone Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D 638 |
Styrolution PS 5400/5401 HIPS Good ESCRHigh ImpactLow gloss (matte finish)USP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF008S PA 66 LNP* THERMOCOMP* RF008S is a compound based on Nylon 6/6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SRF 3704 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: High Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SRP 5608 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: High Gloss; High Impact Resistance Uses: Conduit; Piping; Profiles Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
Total PSI 945 Polystyrene Polystyrene 945 is designed for injection molding applications requiring superior toughness. This polymer is a high impact polystyrene with excellent gloss and falling dart properties. The impact an.. |
|||
Izod Impact, Notched | 1.39 J/cm @Temperature 22.8 °C |
2.60 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger TECANYL™ MT Autoclavable Polymer TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease.. |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
Entec Hyrene® PS-HI 14/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Izod Impact, Notched | 1.39 J/cm | 2.60 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.39 J/cm @Thickness 3.17 mm |
2.60 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Dry) Ultramid 1603-2 NF2004 is a 43% glass reinforced, heat stabilized injection molding nylon 6/6 with the highest level of glass reinforcement for maximum strength and stiffness. |