Polymer Property : Izod Impact, Notched = 1.59 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.290 - 0.850 J/cm
0.543 - 1.59 ft-lb/in
Average value: 0.647 J/cm Grade Count:3
Overview of materials for Nylon 612, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Notched 0.640 - 0.850 J/cm

@Temperature -40.0 - -40.0 °C
1.20 - 1.59 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.745 J/cm Grade Count:2
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Izod Impact, Notched 0.300 - 0.850 J/cm

@Temperature -30.0 - 0.000 °C
0.562 - 1.59 ft-lb/in

@Temperature -22.0 - 32.0 °F
Average value: 0.547 J/cm Grade Count:13
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched 0.850 - 0.850 J/cm

@Temperature -10.0 - 0.000 °C
1.59 - 1.59 ft-lb/in

@Temperature 14.0 - 32.0 °F
Average value: 0.794 J/cm Grade Count:2
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Izod Impact, Notched 0.850 - 0.850 J/cm

@Thickness 3.17 - 6.40 mm
1.59 - 1.59 ft-lb/in

@Thickness 0.125 - 0.252 in
Average value: 0.794 J/cm Grade Count:2
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..