Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.602 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.001 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers 66-41 Nylon 66, Toughened Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.602 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.001 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers ABS-305 Acrylonitrile Butadiene Styrene, General Purpose Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.602 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.001 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers ABS-305LG Acrylonitrile Butadiene Styrene, General Purpose, Low Gloss Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.602 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.001 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers GPCB-330 Polycarbonate+PBT, 30% Glass Fiber Reinforced, Impact Resistant Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.602 J/cm @Thickness 3.17 mm |
3.001 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers GPP-320 Polypropylene, 20% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.602 J/cm @Thickness 3.17 mm |
3.001 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 1.602 J/cm @Thickness 3.17 mm |
3.001 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPP25-1111 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 1.602 J/cm @Thickness 3.17 mm |
3.001 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPP25-1503 GF25 25% Glass Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |