Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.74 J/cm @Temperature 23.0 °C |
3.25 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H5211PBL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE80 pipe, non pressure pipesCertification: Certified by LNEI.. |
|||
Izod Impact, Notched | 1.74 J/cm @Temperature 22.8 °C |
3.25 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger Tecapeek® PVX Polyetheretherketone (PEEK) TECAPEEK® PVX is an ultra high performance bearing material made from Victrex® PEEK polymer. TECAPEEK® PVX incorporates the properties of a premium polymetric matrix material with optimum levels.. |