Material Notes:
TECAPEEK® PVX is an ultra high performance bearing material made from Victrex® PEEK polymer. TECAPEEK® PVX incorporates the properties of a premium polymetric matrix material with optimum levels of specific wear enhancing additives. This formulation raises the continuous use temperature by approximately 40°F and increases the limiting PV while maintaining excellent chemical resistance. When used as a non-metallic bearing, TECAPEEK® PVX offers a good range of tribiological performance. It is designed to run at high loads and speeds, in hostile environments, either dry or lubricated. Continuous use temperature over 450°FFlammability is UL94 V-O with a low limiting O2 index (-40%) and very low smoke generationCan be used dry against hard or soft mating surfacesExcellent weather resistanceResistant to gamma radiationComplies with specific provisions of ASTM D6262-98Available in a wide range of sizes, extruded in rod and plate for subsequent machined parts TECAPEEK® PVX great properties make it an ideal material for bearing surfaces in the most demanding applications and in the harshest conditions. Industrial, automotive, marine, nuclear, petroleum and aerospace industry applications realize great benefits from its use.Information Provided by Ensinger Inc.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Water Absorption <= 0.10 %

@Temperature 22.8 °C,
Time 86400 sec
<= 0.10 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.10 %
0.10 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Tensile Modulus 8.96 GPa
1300 ksi
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
9.65 GPa

@Temperature 22.8 °C
1400 ksi

@Temperature 73.0 °F
Tangent; ASTM D790
Compressive Strength 152 MPa
22000 psi
ASTM D695
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
1.74 J/cm

@Temperature 22.8 °C
3.25 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Coefficient of Friction, Dynamic 0.19

@Pressure 0.276 MPa
0.19

@Pressure 40.0 psi
50 fpm
Coefficient of Friction, Static 0.23

@Pressure 0.276 MPa
0.23

@Pressure 40.0 psi
K Factor (Wear Factor) 1.25 - 1.5
1.25 - 1.5
in/min x 10<sup>-3</sup>
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C
15.0 µin/in-°F
Melting Point 334 °C
633 °F
Maximum Service Temperature, Air 260 °C
500 °F
continuous
Deflection Temperature at 1.8 MPa (264 psi) 277 °C
530 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistivity per Square 1e+05 - 1.00e+8 ohm
1e+05 - 1.00e+8 ohm
ASTM D257
Descriptive Properties Value Comments
Base Material PEEK
Maximum PV 25000-30000