Polymer Property : Izod Impact, Notched = 10.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.374 - 5.34 J/cm
0.700 - 10.0 ft-lb/in
Average value: 0.765 J/cm Grade Count:48
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Izod Impact, Notched 2.40 - 5.34 J/cm
4.50 - 10.0 ft-lb/in
Average value: 3.81 J/cm Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max..
Izod Impact, Notched 0.900 - 5.34 J/cm

@Temperature -40.0 - 0.000 °C
1.69 - 10.0 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 4.02 J/cm Grade Count:18
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 0.900 - 5.34 J/cm

@Thickness 3.17 - 3.20 mm
1.69 - 10.0 ft-lb/in

@Thickness 0.125 - 0.126 in
Average value: 4.02 J/cm Grade Count:18
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 3.74 - 5.34 J/cm
7.00 - 10.0 ft-lb/in
ASTM D256
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Izod Impact, Notched 4.27 - 5.34 J/cm
8.00 - 10.0 ft-lb/in
ASTM D256
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Izod Impact, Notched 4.27 - 5.34 J/cm
8.00 - 10.0 ft-lb/in
ASTM D256
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Izod Impact, Notched 3.74 - 5.34 J/cm
7.00 - 10.0 ft-lb/in
ASTM D256
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound
The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl..
Izod Impact, Notched 4.27 - 5.34 J/cm
8.00 - 10.0 ft-lb/in
ASTM D256
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound
A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Izod Impact, Notched 4.81 - 5.34 J/cm
9.00 - 10.0 ft-lb/in
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant
BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was..
Izod Impact, Notched 2.14 - 5.34 J/cm
4.00 - 10.0 ft-lb/in
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant
BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,..
Izod Impact, Notched 3.74 - 5.34 J/cm
7.00 - 10.0 ft-lb/in
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound
BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a..
Izod Impact, Notched 3.74 - 5.34 J/cm
7.00 - 10.0 ft-lb/in
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound
BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar..
Izod Impact, Notched 4.27 - 5.34 J/cm
8.00 - 10.0 ft-lb/in
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound
BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica..
Izod Impact, Notched 0.910 - 5.34 J/cm
1.70 - 10.0 ft-lb/in
Average value: 3.04 J/cm Grade Count:89
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
Izod Impact, Notched 4.27 - 5.34 J/cm
8.00 - 10.0 ft-lb/in
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound
BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma..