Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typical applications are circuit breakers, insulators, bobbins and electrical connectors.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 2.00 - 2.20 g/cc
0.0723 - 0.0795 lb/in³
Molded
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 40
30 - 40
Tensile Strength 48.3 - 62.1 MPa
7000 - 9000 psi
Flexural Strength 110 - 124 MPa
16000 - 18000 psi
Flexural Modulus 12.4 - 13.8 GPa
1800 - 2000 ksi
Compressive Strength 110 - 138 MPa
16000 - 20000 psi
Izod Impact, Notched 4.27 - 5.34 J/cm
8.00 - 10.0 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 HB
HB
Product is not UL listed.
Electrical Properties Metric English Comments
Dielectric Strength 13.8 - 15.0 kV/mm
350 - 380 kV/in
short time
Arc Resistance >= 183 sec
>= 183 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F
Users viewing this material also viewed the following: