Izod Impact, Notched 10.1 - 10.7 J/cm

@Thickness <=3.00 mm
19.0 - 20.0 ft-lb/in

@Thickness <=0.118 in
ASTM D256A
Plaskolite Mustang PETG Sheet
MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy..
Izod Impact, Notched 0.267 - 10.7 J/cm
0.500 - 20.0 ft-lb/in
Average value: 3.01 J/cm Grade Count:13
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Notched 6.41 - 10.7 J/cm
12.0 - 20.0 ft-lb/in
ASTM D256
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Izod Impact, Notched 5.34 - 10.7 J/cm
10.0 - 20.0 ft-lb/in
ASTM D256
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Izod Impact, Notched 5.34 - 10.7 J/cm
10.0 - 20.0 ft-lb/in
ASTM D256
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Izod Impact, Notched 5.34 - 10.7 J/cm
10.0 - 20.0 ft-lb/in
ASTM D256
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Izod Impact, Notched 0.450 - 10.7 J/cm
0.843 - 20.0 ft-lb/in
Average value: 3.69 J/cm Grade Count:4
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Izod Impact, Notched 0.587 - 10.7 J/cm
1.10 - 20.0 ft-lb/in
Average value: 2.31 J/cm Grade Count:11
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and ..
Izod Impact, Notched 5.34 - 10.7 J/cm
10.0 - 20.0 ft-lb/in
ASTM D256
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..