Izod Impact, Notched 1.30 - 5.70 J/cm

@Temperature -40.0 - -20.0 °C
2.44 - 10.7 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 3.51 J/cm Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Izod Impact, Notched 1.30 - 5.70 J/cm

@Thickness 1.57 - 3.18 mm
2.44 - 10.7 ft-lb/in

@Thickness 0.0618 - 0.125 in
Average value: 3.51 J/cm Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..