Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS (Asia Pacific) CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature 22.8 °C |
11.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature -20.0 °C |
11.0 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature -50.0 °C |
11.0 ft-lb/in @Temperature -58.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature -50.0 °C |
11.0 ft-lb/in @Temperature -58.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Asia Pacific) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Izod Impact, Notched | 5.87 J/cm | 11.0 ft-lb/in | 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid S459HTP ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature 23.0 °C |
11.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature -50.0 °C |
11.0 ft-lb/in @Temperature -58.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature -50.0 °C |
11.0 ft-lb/in @Temperature -58.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® TE5000HZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Handle)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® TE5000LZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provide.. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-1064 PC, Unreinforced FR PC material that is applied to other resin for mobile phone chargersInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® UF-1017B PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-1064 PC, Unreinforced FR PC material that is applied to other resin for mobile phone chargersInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® SC-1220R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.87 J/cm @Temperature 23.0 °C |
11.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Izod Impact, Notched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Asia Pacific) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.20 mm |
11.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® DP 1-1456 Polycarbonate, Impact Grade Impact modified injection molding grade, extremely easy flow and easy mold release, for thin walled applications with long flow lengths.Information provided by Bayer.As of 1 September 2015, Bayer Ma.. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS/PC FC-30 Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABSPC 9901 ELG ABS/PC Injection Molding Grade, Very High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 5.87 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers ASAPC 6141 UV Stabilized Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D256 |
Aclo Accucomp ASA ASA001L |
|||
Izod Impact, Notched | 5.87 J/cm | 11.0 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 520 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1015 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.87 - 6.94 J/cm | 11.0 - 13.0 ft-lb/in | |
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |