Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.785 - 6.00 J/cm | 1.47 - 11.2 ft-lb/in | Average value: 3.05 J/cm Grade Count:40 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.250 - 6.00 J/cm | 0.468 - 11.2 ft-lb/in | Average value: 0.723 J/cm Grade Count:95 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |