Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.05 - 1.52 g/cc
0.0379 - 0.0549 lb/in³
Average value: 1.16 g/cc Grade Count:102
Filler Content 10.0 - 40.0 %
10.0 - 40.0 %
Average value: 26.2 % Grade Count:26
Water Absorption 0.0100 - 0.300 %
0.0100 - 0.300 %
Average value: 0.0550 % Grade Count:30
Linear Mold Shrinkage 0.00100 - 0.0150 cm/cm
0.00100 - 0.0150 in/in
Average value: 0.00457 cm/cm Grade Count:96
Linear Mold Shrinkage, Transverse 0.00500 - 0.00900 cm/cm
0.00500 - 0.00900 in/in
Average value: 0.00770 cm/cm Grade Count:5
Melt Flow 1.00 - 30.0 g/10 min
1.00 - 30.0 g/10 min
Average value: 6.99 g/10 min Grade Count:66
Ash 30.0 - 35.0 %
30.0 - 35.0 %
Average value: 30.2 % Grade Count:26
Mechanical Properties Metric English Comments
Hardness, Rockwell M 53.0 - 70.0
53.0 - 70.0
Average value: 64.0 Grade Count:3
Hardness, Rockwell R 40.0 - 117
40.0 - 117
Average value: 88.3 Grade Count:52
Hardness, Shore D 73.0 - 79.0
73.0 - 79.0
Average value: 75.4 Grade Count:14
Tensile Strength, Ultimate 20.0 - 150 MPa
2900 - 21800 psi
Average value: 50.1 MPa Grade Count:83
9.00 - 80.0 MPa

@Temperature 60.0 - 120 °C
1310 - 11600 psi

@Temperature 140 - 248 °F
Average value: 31.0 MPa Grade Count:2
Tensile Strength, Yield 20.0 - 75.8 MPa
2900 - 11000 psi
Average value: 47.2 MPa Grade Count:46
Elongation at Break 1.00 - 37.0 %
1.00 - 37.0 %
Average value: 6.20 % Grade Count:66
2.90 - 2.90 %

@Temperature 80.0 - 80.0 °C
2.90 - 2.90 %

@Temperature 176 - 176 °F
Average value: 2.90 % Grade Count:1
Elongation at Yield 2.30 - 100 %
2.30 - 100 %
Average value: 8.26 % Grade Count:32
Modulus of Elasticity 2.40 - 12.3 GPa
348 - 1780 ksi
Average value: 4.64 GPa Grade Count:45
8.80 - 8.80 GPa

@Temperature 80.0 - 80.0 °C
1280 - 1280 ksi

@Temperature 176 - 176 °F
Average value: 8.80 GPa Grade Count:1
Flexural Yield Strength 31.0 - 220 MPa
4500 - 31900 psi
Average value: 77.7 MPa Grade Count:74
120 - 120 MPa

@Temperature 80.0 - 80.0 °C
17400 - 17400 psi

@Temperature 176 - 176 °F
Average value: 120 MPa Grade Count:1
Flexural Modulus 1.88 - 11.4 GPa
273 - 1650 ksi
Average value: 4.43 GPa Grade Count:104
0.600 - 7.80 GPa

@Temperature 60.0 - 120 °C
87.0 - 1130 ksi

@Temperature 140 - 248 °F
Average value: 3.05 GPa Grade Count:2
Compressive Yield Strength 39.3 - 62.1 MPa
5700 - 9000 psi
Average value: 50.7 MPa Grade Count:7
Izod Impact, Notched 0.250 - 6.00 J/cm
0.468 - 11.2 ft-lb/in
Average value: 0.723 J/cm Grade Count:95
0.250 - 2.00 J/cm

@Temperature -40.0 - 0.000 °C
0.468 - 3.75 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 1.09 J/cm Grade Count:3
2.1356 - 2.1356 J/cm

@Temperature -28.9 - -28.9 °C
4.0009 - 4.0009 ft-lb/in

@Temperature -20.0 - -20.0 °F
Average value: 1.09 J/cm Grade Count:1
2.1356 - 2.1356 J/cm

@Thickness 3.17 - 3.17 mm
4.0009 - 4.0009 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.09 J/cm Grade Count:1
Izod Impact, Unnotched 1.60 - 7.47 J/cm
3.00 - 14.0 ft-lb/in
Average value: 3.76 J/cm Grade Count:34
Izod Impact, Notched (ISO) 5.00 - 7.80 kJ/m²
2.38 - 3.71 ft-lb/in²
Average value: 5.53 kJ/m² Grade Count:6
3.70 - 4.70 kJ/m²

@Temperature -40.0 - -40.0 °C
1.76 - 2.24 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 4.03 kJ/m² Grade Count:4
Charpy Impact Unnotched 1.80 - 7.80 J/cm²
8.57 - 37.1 ft-lb/in²
Average value: 4.03 J/cm² Grade Count:4
1.00 - 7.20 J/cm²

@Temperature -40.0 - -20.0 °C
4.76 - 34.3 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.07 J/cm² Grade Count:2
Charpy Impact, Notched 0.800 - 3.70 J/cm²
3.81 - 17.6 ft-lb/in²
Average value: 1.90 J/cm² Grade Count:3
0.500 - 3.90 J/cm²

@Temperature -30.0 - -20.0 °C
2.38 - 18.6 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 2.20 J/cm² Grade Count:2
Gardner Impact 0.339 - 4.52 J
0.250 - 3.33 ft-lb
Average value: 0.693 J Grade Count:22
Thermal Properties Metric English Comments
CTE, linear 21.6 - 51.0 µm/m-°C
12.0 - 28.3 µin/in-°F
Average value: 39.9 µm/m-°C Grade Count:15
Thermal Conductivity 0.303 - 0.360 W/m-K
2.10 - 2.50 BTU-in/hr-ft²-°F
Average value: 0.336 W/m-K Grade Count:9
Melting Point 163 - 182 °C
325 - 360 °F
Average value: 171 °C Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 133 - 169 °C
271 - 336 °F
Average value: 152 °C Grade Count:91
Deflection Temperature at 1.8 MPa (264 psi) 35.6 - 155 °C
96.0 - 311 °F
Average value: 122 °C Grade Count:93
Vicat Softening Point 55.0 - 160 °C
131 - 320 °F
Average value: 111 °C Grade Count:6
Flammability, UL94 HB
HB
Grade Count:31
Oxygen Index 21.0 %
21.0 %
Average value: 21.0 % Grade Count:3
Glow Wire Test 650 - 750 °C
1200 - 1380 °F
Average value: 683 °C Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 - 1.00e+17 ohm-cm
1.00e+15 - 1.00e+17 ohm-cm
Average value: 2.97e+16 ohm-cm Grade Count:16
Dielectric Constant 2.50 - 3.50
2.50 - 3.50
Average value: 2.94 Grade Count:11
Dielectric Strength 19.7 - 30.0 kV/mm
500 - 762 kV/in
Average value: 22.5 kV/mm Grade Count:15
Dissipation Factor 0.00200 - 0.00600
0.00200 - 0.00600
Average value: 0.00286 Grade Count:7
Arc Resistance 120 - 130 sec
120 - 130 sec
Average value: 125 sec Grade Count:11
Processing Properties Metric English Comments
Processing Temperature 30.0 - 270 °C
86.0 - 518 °F
Average value: 208 °C Grade Count:20
Nozzle Temperature 54.4 - 243 °C
130 - 470 °F
Average value: 220 °C Grade Count:27
Melt Temperature 190 - 270 °C
374 - 518 °F
Average value: 225 °C Grade Count:38
Mold Temperature 26.7 - 90.0 °C
80.0 - 194 °F
Average value: 46.7 °C Grade Count:51