Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.50 J/cm @Temperature 23.0 °C |
12.2 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Mytex Polymers AS66K-01 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Izod Impact, Notched | 6.51 J/cm | 12.2 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by .. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Ovation Polymers Nima™ NH PC151 Polycarbonate Non-Hal FR-PC with High HDT, high impact and improved processability. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared accordi.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2203-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Excellent stiffness to weight rat.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 915AU PC (Asia Pacific) LEXAN resin grade 915AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in transparent colors, inte.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -30.0 °C |
12.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 923X PC (Asia Pacific) Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -30.0 °C |
12.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific) Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -30.0 °C |
12.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 9931X PC (Europe-Africa-Middle East) Lexan* 9931X is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperatu.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -40.0 °C |
12.2 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8134 PC COPOLYMER (Asia Pacific) Lexan* EXL8134 is a PC/siloxane copolymer resin with high flow, excellent low temperature impact and 30% post consumer recycle content. Limited availability and restricted color only. Higher color v.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -40.0 °C |
12.2 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8454 PC COPOLYMER (Asia Pacific) Lexan* EXL8454 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 50% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -30.0 °C |
12.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8483 PC COPOLYMER (Asia Pacific) Lexan* EXL8483 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 80% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Reliance Industries Reclair ER-19 Reclair ER-19 is a Octene Conomer based medium density Polyethylene grade designed for Rotational Molding applications with optimum loading of UV Stabilizer. Processing is similar to Butene grades... |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL N145-02 General Purpose POM, Unreinforced, Externally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL N145-AS Antistatic POM, Unreinforced, Internally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL VC-145 Antistatic POM, Unreinforced, Ultra High Flow, For VCR Reels LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
LG Chemical LUCEL FW-700A Friction and Wear Resistant POM, Polymeric Wear Additive LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SPS Guang Zhou POLOYâ„¢ 2001(+) PC/ABS Characteristic: Good mechanical properties and good machining propertiesApplications: Electron equipment shell, automobile assorted partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Eastman Tritan MX810 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Eastman Tritan TX2001 Copolyester Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® G70A4 Impact Resistance at Low Temperature PC/ABS Alloy Impact Resistance at Low TemperatureInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 6.51 J/cm | 12.2 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437C10L1 Calcium Reinforced |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML1661 PC Copolymer (Asia Pacific) Medium-flow impact-modified light-shielding high-flow-ductile PC copolymer. Available in white color only. |