Reliance Industries Reclair ER-19

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Reclair ER-19.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reclair ER-19 is a Octene Conomer based medium density Polyethylene grade designed for Rotational Molding applications with optimum loading of UV Stabilizer. Processing is similar to Butene grades. Excellent toughness and ESCR.Information provided by Reliance Industries
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D368
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
Izod Impact, Notched 6.50 J/cm
12.2 ft-lb/in
ASTM D256