Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
NYCOA 7551 Copolymer Nylon Alloy resistant to zinc chloride and other automotive fluids, good adhesion to olefins, mold & extrusion.Information provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature 23.0 °C |
12.2 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Mytex Polymers AS66K-01 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Ovation Polymers Nima™ NH PC151 Polycarbonate Non-Hal FR-PC with High HDT, high impact and improved processability. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared accordi.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2205-20 CRSX Polyester SMC Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, we.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 915AU PC LEXAN resin grade 915AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in transparent colors, inte.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 915AU PC (Asia Pacific) LEXAN resin grade 915AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in transparent colors, inte.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -30.0 °C |
12.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 923X PC (Asia Pacific) Lexan*923x is a UV stabilized high flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low temperatur.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -30.0 °C |
12.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -30.0 °C |
12.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific) Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -40.0 °C |
12.2 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8134 PC COPOLYMER (Asia Pacific) Lexan* EXL8134 is a PC/siloxane copolymer resin with high flow, excellent low temperature impact and 30% post consumer recycle content. Limited availability and restricted color only. Higher color v.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -40.0 °C |
12.2 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8454 PC COPOLYMER (Asia Pacific) Lexan* EXL8454 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 50% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Izod Impact, Notched | 6.50 J/cm @Temperature -30.0 °C |
12.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8483 PC COPOLYMER (Asia Pacific) Lexan* EXL8483 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 80% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Reliance Industries Reclair ER-19 Reclair ER-19 is a Octene Conomer based medium density Polyethylene grade designed for Rotational Molding applications with optimum loading of UV Stabilizer. Processing is similar to Butene grades... |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL N145-02 General Purpose POM, Unreinforced, Externally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL N145-AS Antistatic POM, Unreinforced, Internally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
LG Chemical LUCEL FW-700A Friction and Wear Resistant POM, Polymeric Wear Additive LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Eastman Tritan MX810 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Eastman Tritan MX811 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceGood heat resistanceO.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Eastman Tritan TX2000 Copolyester Eastman Tritan TX2000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
Eastman Tritan TX2001 Copolyester Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |
|||
Izod Impact, Notched | 6.50 J/cm | 12.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML1661 PC Copolymer (Asia Pacific) Medium-flow impact-modified light-shielding high-flow-ductile PC copolymer. Available in white color only. |