Polymer Property : Izod Impact, Notched = 12.9 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.179 - 12.9 J/cm
0.335 - 24.2 ft-lb/in
Average value: 3.51 J/cm Grade Count:95
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..