Izod Impact, Notched 0.179 - 12.9 J/cm
0.335 - 24.2 ft-lb/in
Average value: 3.51 J/cm Grade Count:95
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
Izod Impact, Notched >= 0.179 J/cm
>= 0.335 ft-lb/in
Method A; ASTM D 256
Karina E 858-10/16-ERYA PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched 0.179 J/cm
0.335 ft-lb/in
ASTM D256
Plenco 7507 Phenolic, Granular, Injection Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..