Polymer Property : Izod Impact, Notched = 2.49 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.960 - 1.33 J/cm

@Thickness 6.35 mm
1.80 - 2.49 ft-lb/in

@Thickness 0.250 in
ASTM D256
PolyOne Lubri-Tech™ PS-30GF/ 02S PBT Polyester - 30% Glass Fiber - 2% Silicone  (discontinued **)
Data provided by PolyOne.
Izod Impact, Notched 0.160 - 1.33 J/cm
0.300 - 2.49 ft-lb/in
Average value: 0.545 J/cm Grade Count:22
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Notched 0.800 - 1.33 J/cm

@Thickness 6.35 mm
1.50 - 2.49 ft-lb/in

@Thickness 0.250 in
ASTM D256
PolyOne Edgetek® MP-10GF/000 Modified PPO - 10% Glass Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Izod Impact, Notched 0.800 - 1.33 J/cm

@Thickness 6.35 mm
1.50 - 2.49 ft-lb/in

@Thickness 0.250 in
ASTM D256
PolyOne Lubri-Tech™ AS-000/10T-2S ABS - 10% PTFE - 2% Silicone  (discontinued **)
Data provided by PolyOne.