Mechanical Properties Metric English Comments
Izod Impact, Notched 1.86865 - 2.6695 J/cm

@Temperature -40.0 - -17.8 °C
3.50075 - 5.0011 ft-lb/in

@Temperature -40.0 - 0.000 °F
Average value: 2.22 J/cm Grade Count:2
Overview of materials for Polyphenylene Ether, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.80085 - 2.6695 J/cm

@Temperature -29.0 - -28.9 °C
1.5003 - 5.0011 ft-lb/in

@Temperature -20.2 - -20.0 °F
Average value: 1.43 J/cm Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max..
Izod Impact, Notched 0.5339 - 2.6695 J/cm

@Temperature -40.0 - 72.8 °C
1.000 - 5.0011 ft-lb/in

@Temperature -40.0 - 163 °F
Average value: 1.51 J/cm Grade Count:18
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.5339 - 2.6695 J/cm

@Thickness 3.17 - 3.17 mm
1.000 - 5.0011 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.51 J/cm Grade Count:18
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.5339 - 2.6695 J/cm

@Temperature -40.0 - -40.0 °C
1.000 - 5.0011 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.29 J/cm Grade Count:16
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Notched 0.5339 - 2.6695 J/cm

@Thickness 3.17 - 3.17 mm
1.000 - 5.0011 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.29 J/cm Grade Count:16
Overview of materials for Nylon 66, Heat Stabilized