Overview of materials for Polyphenylene Ether, Impact Grade

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Impact Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyphenylene Ether, Impact Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.04 - 1.24 g/cc
0.0376 - 0.0448 lb/in³
Average value: 1.10 g/cc Grade Count:8
Water Absorption 0.0700 - 0.100 %
0.0700 - 0.100 %
Average value: 0.0850 % Grade Count:4
Linear Mold Shrinkage 0.00500 - 0.00700 cm/cm
0.00500 - 0.00700 in/in
Average value: 0.00600 cm/cm Grade Count:8
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.5 - 74.0 MPa
5000 - 10700 psi
Average value: 54.2 MPa Grade Count:7
Tensile Strength, Yield 34.5 - 46.9 MPa
5000 - 6800 psi
Average value: 42.1 MPa Grade Count:3
Elongation at Break 30.0 - 70.0 %
30.0 - 70.0 %
Average value: 50.0 % Grade Count:3
Flexural Yield Strength 48.3 - 110 MPa
7000 - 16000 psi
Average value: 84.8 MPa Grade Count:6
Flexural Modulus 1.76 - 3.40 GPa
255 - 493 ksi
Average value: 2.41 GPa Grade Count:8
Izod Impact, Notched 1.55 - 4.27 J/cm
2.90 - 8.00 ft-lb/in
Average value: 2.82 J/cm Grade Count:8
1.86865 - 2.6695 J/cm

@Temperature -40.0 - -17.8 °C
3.50075 - 5.0011 ft-lb/in

@Temperature -40.0 - 0.000 °F
Average value: 2.22 J/cm Grade Count:2
Izod Impact, Notched (ISO) 14.7 - 14.7 kJ/m²

@Temperature -30.0 - -30.0 °C
6.99 - 6.99 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 14.7 kJ/m² Grade Count:1
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 - 157 °C
210 - 315 °F
Average value: 122 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 93.3 - 149 °C
200 - 300 °F
Average value: 110 °C Grade Count:8