Polymer Property : Izod Impact, Notched = 0.5339 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.5339 J/cm
1.000 ft-lb/in
ASTM D256
RedEye On Demand PC-ISO for Parts that can be Sterilized
Polycarbonate-ISO (PC-ISO) is a durable high-performance plastic that meets both ISO 10993-1 and USP Class VI standards in its raw state. PC-ISO can be sterilized using either the gamma radiation or..
Izod Impact, Notched 0.5339 - 1.0678 J/cm

@Temperature -40.0 - -30.0 °C
1.000 - 2.0004 ft-lb/in

@Temperature -40.0 - -22.0 °F
Average value: 0.774 J/cm Grade Count:4
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
Izod Impact, Notched 0.5339 - 1.01441 J/cm

@Temperature -40.0 - 0.000 °C
1.000 - 1.90041 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.774 J/cm Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a..
Izod Impact, Notched 0.5339 - 1.01441 J/cm

@Thickness 3.17 - 3.17 mm
1.000 - 1.90041 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.774 J/cm Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a..
Izod Impact, Notched 0.5339 - 2.50 J/cm

@Temperature -40.0 - 0.000 °C
1.000 - 4.68 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 1.05 J/cm Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Izod Impact, Notched 0.5339 - 2.50 J/cm

@Thickness 3.17 - 6.35 mm
1.000 - 4.68 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 1.05 J/cm Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Izod Impact, Notched 0.5339 - 2.6695 J/cm

@Temperature -40.0 - 72.8 °C
1.000 - 5.0011 ft-lb/in

@Temperature -40.0 - 163 °F
Average value: 1.51 J/cm Grade Count:18
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.5339 - 2.6695 J/cm

@Thickness 3.17 - 3.17 mm
1.000 - 5.0011 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.51 J/cm Grade Count:18
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 0.5339 - 2.6695 J/cm

@Temperature -40.0 - -40.0 °C
1.000 - 5.0011 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.29 J/cm Grade Count:16
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Notched 0.5339 - 2.6695 J/cm

@Thickness 3.17 - 3.17 mm
1.000 - 5.0011 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.29 J/cm Grade Count:16
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Notched 0.5339 - 0.5339 J/cm

@Temperature -40.0 - -40.0 °C
1.000 - 1.000 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.534 J/cm Grade Count:1
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Izod Impact, Notched 0.5339 - 0.5339 J/cm

@Thickness 3.17 - 3.17 mm
1.000 - 1.000 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.534 J/cm Grade Count:1
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Izod Impact, Notched 0.5339 J/cm
1.000 ft-lb/in
ASTM D256
Stratasys® Polycarbonate
A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts ..
Izod Impact, Notched 0.5339 J/cm
1.000 ft-lb/in
ASTM D256
Stratasys® Polycarbonate-ISO
PC-ISO (polycarbonate-ISO), an industrial thermoplastic, in its raw state meets the ISO 10993-1 and USP Class VI classification1 and comes in a variety of colors. Because of their strength and medic..
Izod Impact, Notched 0.5339 - 0.90763 J/cm

@Temperature -40.0 - -30.0 °C
1.000 - 1.7004 ft-lb/in

@Temperature -40.0 - -22.0 °F
Average value: 0.692 J/cm Grade Count:3
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Izod Impact, Notched 0.5339 - 0.74746 J/cm

@Temperature -40.0 - -30.0 °C
1.000 - 1.4003 ft-lb/in

@Temperature -40.0 - -22.0 °F
Average value: 0.641 J/cm Grade Count:2
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Izod Impact, Notched 0.5339 - 3.50 J/cm

@Temperature -40.0 - 0.000 °C
1.000 - 6.56 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 1.23 J/cm Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Izod Impact, Notched 0.5339 - 0.5339 J/cm

@Temperature -28.9 - -28.9 °C
1.000 - 1.000 ft-lb/in

@Temperature -20.0 - -20.0 °F
Average value: 0.533 J/cm Grade Count:1
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Izod Impact, Notched 0.5339 - 0.5339 J/cm

@Thickness 3.17 - 3.17 mm
1.000 - 1.000 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.533 J/cm Grade Count:1
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Izod Impact, Notched 0.5339 - 0.5339 J/cm

@Temperature -28.9 - -28.9 °C
1.000 - 1.000 ft-lb/in

@Temperature -20.0 - -20.0 °F
Average value: 1.55 J/cm Grade Count:1
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..
Izod Impact, Notched 0.5339 - 0.5339 J/cm

@Thickness 3.17 - 3.17 mm
1.000 - 1.000 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.55 J/cm Grade Count:1
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..
Copyright © lookpolymers.com All Rights Reserved