Izod Impact, Notched 0.550 - 3.80 J/cm

@Temperature -30.0 - 0.000 °C
1.03 - 7.12 ft-lb/in

@Temperature -22.0 - 32.0 °F
Average value: 1.52 J/cm Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..