Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.0678 - 2.1356 J/cm @Temperature -40.0 - -20.0 °C |
2.0004 - 4.0009 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 1.51 J/cm Grade Count:2 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Izod Impact, Notched | 1.0678 - 2.1356 J/cm @Thickness 3.17 - 3.17 mm |
2.0004 - 4.0009 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.51 J/cm Grade Count:2 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Izod Impact, Notched | 2.1356 - 2.1356 J/cm @Temperature -40.0 - -30.0 °C |
4.0009 - 4.0009 ft-lb/in @Temperature -40.0 - -22.0 °F |
Average value: 3.16 J/cm Grade Count:3 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | 2.1356 - 2.1356 J/cm @Thickness 3.17 - 3.20 mm |
4.0009 - 4.0009 ft-lb/in @Thickness 0.125 - 0.126 in |
Average value: 3.16 J/cm Grade Count:3 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched | 2.1356 - 2.1356 J/cm @Temperature -28.9 - -28.9 °C |
4.0009 - 4.0009 ft-lb/in @Temperature -20.0 - -20.0 °F |
Average value: 1.09 J/cm Grade Count:1 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 2.1356 - 2.1356 J/cm @Thickness 3.17 - 3.17 mm |
4.0009 - 4.0009 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.09 J/cm Grade Count:1 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |