Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.41 J/cm | 10.1 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620 PP SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was origin.. |