Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 9.10 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 9.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
17.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ 1010 A Black 13 Polyamide 6 (Nylon 6)
The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of ..
Izod Impact, Notched 9.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
17.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ 2024 HS UV 425C Grey Polyamide 66 (Nylon 66)
The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range o..
Izod Impact, Notched 9.10 J/cm

@Thickness 3.20 mm
17.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade  (discontinued **)
Pseudoplastic behavior and high viscosity extrusion and injection molding grade, BgVV- and FDA grade for food contact applications, high melt stability, better resistance to hot water, specially sui..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256; ISO 180/4A
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 2060-6 Polycarbonate Resin
Overview: CALIBRE™ 2060-6 polycarbonate resin is used in medical applications involving steam or ethylene oxide sterilization – through suitability for use in these applications is depende..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 301V-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 301V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 301V-6 contains a mold release agent and is..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ISO 180/4A
Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are avai..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 300-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 a..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 300-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-6 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity as high melt strength for blow molding and sheet applications. ..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 302-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 302-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, and optical clarity as well as high melt strength for blow molding and sheet appli..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 302V-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 302V-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity (for tinted/transparent colors), and is available in both tint..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 303V-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 303V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 303V-6 contains a mold release agent, a UV ..
Izod Impact, Notched 9.10 J/cm

@Thickness 3.20 mm
17.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Makrolon® 2605 Polycarbonate, Injection Grade
Easy flowing injection molding grade with easy mold release, Makrolon grade 2658 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat..
Izod Impact, Notched 9.10 J/cm

@Thickness 3.20 mm
17.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Makrolon® 2607 Polycarbonate, Injection Grade
Easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially a..
Izod Impact, Notched 9.10 J/cm

@Thickness 3.20 mm
17.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Makrolon® 2658 Polycarbonate, Injection Grade
Easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer M..
Izod Impact, Notched 9.10 J/cm

@Thickness 3.20 mm
17.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Makrolon® 2805 Polycarbonate, Injection Grade
Medium flowing injection molding grade with easy mold release, Makrolon grade 2858 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separ..
Izod Impact, Notched 9.10 J/cm

@Thickness 3.20 mm
17.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Makrolon® 2858 Polycarbonate, Injection Grade
Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se..
Izod Impact, Notched 9.10 J/cm
17.0 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 827LD Nylon 6
A very high impact nylon resin for injection molding applications. Outstanding low temperature properties.Data provided by the manufacturer
Copyright © lookpolymers.com All Rights Reserved