Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.181 J/cm² @Temperature 0.000 °C |
0.860 ft-lb/in² @Temperature 32.0 °F |
ISO 179 |
ExxonMobil Exxtral™ LNU 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with high stiffness, high gloss, low discoloration and good detergent resistance for large electrical appliances such as washing machi.. |