Polymer Property : Charpy Impact, Notched = 0.860 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.181 J/cm²

@Temperature 0.000 °C
0.860 ft-lb/in²

@Temperature 32.0 °F
ISO 179
ExxonMobil Exxtral™ LNU 011 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with high stiffness, high gloss, low discoloration and good detergent resistance for large electrical appliances such as washing machi..