Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.340 J/cm² @Temperature 23.0 °C |
1.62 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A CP400 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.340 J/cm² @Temperature -30.0 °C |
1.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® S650FR BK851 PBT
(Unverified Data**) Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.340 J/cm² @Temperature -30.0 °C |
1.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Solvay TECHNYL® C 52G1 V20 PA6, Conditioned Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North Amer.. |
|||
Charpy Impact, Notched | 0.340 J/cm² @Temperature 23.0 °C |
1.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Charpy Impact, Notched | 0.340 J/cm² @Temperature -30.0 °C |
1.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Charpy Impact, Notched | 0.340 J/cm² @Temperature 23.0 °C |
1.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |