Polymer Property : Charpy Impact, Notched = 1.05 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.220 J/cm²

@Temperature -20.0 °C
1.05 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 GB 30 PA6, 30% glass beads
FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti..
Charpy Impact, Notched 0.220 J/cm²

@Temperature -20.0 °C
1.05 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 GB 30 TS PA6, 30% glass beads
FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti..
Charpy Impact, Notched 0.220 J/cm²

@Temperature -30.0 °C
1.05 ft-lb/in²

@Temperature -22.0 °F
Radici Radiflam® S FR (cond.) Nylon 6
PA6 flame retardant injection molding grade. Halogen and phosphorus free. Natural color. Suitable for monofilament extrusion.Information provided by Radici group.
Charpy Impact, Notched 0.220 J/cm²

@Temperature 23.0 °C
1.05 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-2140 BLH 40% Talc-Filled Polypropylene Homopolymer
INNOPOL® CS 1-2140 BLH is recommended especially for producing products, where high stiffness, low shrinkage, long term heat stability and excellent processability are required.All information pr..
Charpy Impact, Notched 0.220 J/cm²

@Temperature -20.0 °C
1.05 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend
INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 3-9..
Charpy Impact, Notched 0.220 J/cm²

@Temperature -30.0 °C
1.05 ft-lb/in²

@Temperature -22.0 °F
Radici Radiflam® A AE (cond.) Nylon 66
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g..