Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radiflam® A AE (cond.) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® A AE (cond.) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
(Dry)
Water Absorption 6.2 %
6.2 %
initially dry
Moisture Absorption at Equilibrium 1.6 %
1.6 %
initially dry
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
Elongation at Break 3.2 %
3.2 %
Tensile Modulus 2.30 GPa
334 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 0.220 J/cm²

@Temperature -30.0 °C
1.05 ft-lb/in²

@Temperature -22.0 °F
0.330 J/cm²

@Temperature 23.0 °C
1.57 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 350 V
350 V