Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.240 J/cm²

@Temperature -30.0 °C
1.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179
PolyOne Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6)
Information provided by PolyOne
Charpy Impact, Notched 0.240 J/cm²

@Temperature 23.0 °C
1.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
PolyOne Bergamid™ B70 GK/Mi30 BK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Charpy Impact, Notched 0.240 J/cm²

@Temperature -20.0 °C
1.14 ft-lb/in²

@Temperature -4.00 °F
LATI Latene® 7H2W T-V0 PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardantsAvailability: Africa & Middle East; Asia Pacif..
Charpy Impact, Notched 0.240 J/cm²

@Temperature -30.0 °C
1.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Borealis Daplen™ EF341AE Polypropylene TPO Compound
Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
Charpy Impact, Notched 0.240 J/cm²

@Temperature -20.0 °C
1.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis ME268Al Polypropylene Compound, Mineral Filled
ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par..