Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C3100 PC+ABS (Europe-Africa-Middle East) C3100 is blow moulding/extrusion grade offering low temperature ductility, high heat resistance and high meltstrength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYblend 65CI PC/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 65FS LB PC/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 65FS PC/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 65H PC/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 85V PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Thickness 102 mm, Temperature -20.0 °C |
19.0 ft-lb/in² @Thickness 4.00 in, Temperature -4.00 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Thickness 102 mm, Temperature 23.0 °C |
19.0 ft-lb/in² @Thickness 4.00 in, Temperature 73.4 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East) High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYlux 4010 MP PC/PBT-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A52^E Nylon 66, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANBLEND FS7 FR UV PC/ASA Blend, Flame-Retardant, UV Stabilized Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Lexan® ML3041 PC (Europe-Africa-Middle East) LEXAN ML3041 has been developed for the injection moulding of thin-wall, complex parts that require high mechanical properties and impact resistance.This data was supplied by SABIC-IP for the Europe.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 406 FD C CM 406 Polycarbonate/ABS Blend (European Grade) Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Luran® S 797 S White 35962 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® 4105 ABS Novodur Ultra 4105 is a PC modified high heat injection molding grade with high impact strength.Information provided by Styrolution |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Borpact™ BC918CF Polypropylene Copolymer Borpact™ BC918CF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. Optical properties will not be deteriorated as with conventional homo or .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 2006 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-PG6 Impact Modified Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® CL101D PBT+PC (Europe-Africa-Middle East) XENOY CL101D is an impact modified PBT+PC injection moulding resin with excellent low temperature impact performance. Applications: automotive exterior components such as bumper systems.This data wa.. |