Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 65FS LB PC/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 85V PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Thickness 102 mm, Temperature -20.0 °C |
19.0 ft-lb/in² @Thickness 4.00 in, Temperature -4.00 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A52^E Nylon 66, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -20.0 °C |
19.0 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A53^E Nylon 66, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANTEC PC M75R Polycarbonate, Steam Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANTEC PC S60R Polycarbonate Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Lexan® ML3041 PC (Europe-Africa-Middle East) LEXAN ML3041 has been developed for the injection moulding of thin-wall, complex parts that require high mechanical properties and impact resistance.This data was supplied by SABIC-IP for the Europe.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical PI-642 ABS, Fitting, High Strength Information Provided by LG Chem |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-2000 TO Polypropylene Block-Copolymer Based Compound INNOPOL® CS 2-2000 TO is a polypropylene block-copolymer based compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-2000 TO is developed for producing injection m.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-5000 Polypropylene Block-Copolymer INNOPOL® CS 2-5000 is a polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-5000 is developed for producing injection molded automot.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 406 FD C CM 406 Polycarbonate/ABS Blend (European Grade) Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 406 FD Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® CL402U PBT+PC (Europe-Africa-Middle East) XENOY CL402U has been specially developed for extrusion blowmoulding applications, where higher melt strength is desired. XENOY CL402U is a high impact material combined with good UV resistance perf.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East) XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Luran® S 797 S White 35962 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® 4105 ABS Novodur Ultra 4105 is a PC modified high heat injection molding grade with high impact strength.Information provided by Styrolution |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 2002 25% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 2006 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Mitsubishi Xantar® C CM 506 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |