Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.650 J/cm² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH GF5020 HC Polypropylene Homopolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A RV150 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® CE15330 BK010 PBT
(Unverified Data**) Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 911DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-2120 17TOP BU UV-Stabilized 17% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2120 17TOP BU is a black colored, 17% talc-filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-2120 17TOP BU is developed for producing injection .. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-5000 Polypropylene Block-Copolymer INNOPOL® CS 2-5000 is a polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-5000 is developed for producing injection molded automot.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1A |
Gromax BTE25-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | >= 0.650 J/cm² @Temperature 23.0 °C |
>= 3.09 ft-lb/in² @Temperature 73.4 °F |
edgewise; ISO 179 |
MTM Plastics Dipolen® S Recycled PP + PE Blend Dipolen® S is a granulated polyolefin blend for use in either extrusion or injection molding. It can be supplied unmodified or treated with additives according to customer specifications. Dipole.. |
|||
Charpy Impact, Notched | >= 0.650 J/cm² @Temperature 23.0 °C |
>= 3.09 ft-lb/in² @Temperature 73.4 °F |
edgewise; ISO 179 |
MTM Plastics Purpolen® PP Polypropylene Regrind Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® .. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
|
LATI Lapex A PES Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Daplen™ EF267AI Polypropylene TPO Compound Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Novamid® 1010GN2-15Z BK701 PA6-GF15 FR(17) 15% Glass Reinforced, Flame Retardant, Easy Molding Grade, Injection Molding, High Flow |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eA |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultraform® N2200 G43 POM Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultraform® N2320 0035 LEV POM Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultraform® N2640 E2 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with enhanced toughness and high weld line strength.Information provided by BASF |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |