Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.651 J/cm² @Temperature -20.0 °C |
3.10 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
ExxonMobil Exxtral™ BMU 233 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact, good dimensional stability and good UV resistance.Availability.. |
|||
Charpy Impact, Notched | 0.651 J/cm² @Temperature 0.000 °C |
3.10 ft-lb/in² @Temperature 32.0 °F |
ISO 179 |
ExxonMobil Exxtral™ CNR 012 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive applications. Availability: Africa & Middle East, Asia Pacific, Europe South America and Nort.. |
|||
Charpy Impact, Notched | 0.651 J/cm² @Temperature 0.000 °C |
3.10 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CNU 015 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good stiffness/toughness balance, low odor and emissions, designed for automotive interior applications. Availability: Africa & M.. |