Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 25.5 J/cm² - NB | 121 ft-lb/in² - NB | Average value: 26.5 J/cm² Grade Count:8 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Charpy Impact Unnotched | 25.5 J/cm² | 121 ft-lb/in² | |
Arkema Group Kynar® 4000 HD PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b.. |