Mechanical Properties Metric English Comments
Charpy Impact Unnotched 25.5 J/cm² - NB
121 ft-lb/in² - NB
Average value: 26.5 J/cm² Grade Count:8
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Charpy Impact Unnotched 25.5 J/cm²
121 ft-lb/in²
Arkema Group Kynar® 4000 HD PVDF  (discontinued **)
Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b..