Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.30 J/cm² @Temperature -40.0 °C |
10.9 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature -40.0 °C |
10.9 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 W-KF30 Nylon 6 for injection molding, 30% short glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.30 - 8.00 J/cm² | 10.9 - 38.1 ft-lb/in² | Average value: 4.42 J/cm² Grade Count:44 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 2.30 J/cm² - NB | 10.9 ft-lb/in² - NB | Average value: 5.37 J/cm² Grade Count:20 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 2.30 - 6.80 J/cm² | 10.9 - 32.4 ft-lb/in² | Average value: 4.31 J/cm² Grade Count:17 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 CV-CU 0550 Nylon 6.6 for injection molding, 5% carbon fiber reinforced, 50% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.30 - 9.00 J/cm² | 10.9 - 42.8 ft-lb/in² | Average value: 5.30 J/cm² Grade Count:10 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature -30.0 °C |
10.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 20-7314 Polyphthalamide, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature -30.0 °C |
10.9 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | EN ISO 179/1eU |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
Charpy Impact Unnotched | 2.30 J/cm² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179; DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1400T (PET + solid lubricant) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL BK083 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addilene PMD 50272 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179-1eU |
Barlog Plastics KEBATRON C2065X3 PPS, cross-linked, 65% glass fiber / mineral reinforced, reduced residual chlorine PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | |
BASF Polystyrol® 165 H Polystyrene (Europe) High molecular grades, often blended with high-impact extrusion grades (e.g. for dairy products).Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | |
Arkema Group Appryl® HXN 1240 Polypropylene, 40% Talc Filled Compound of a PP homopolymer and 40% talc, warm stabilized suitable for under hood automotive applications.ISO data provided by the manufacturer, Arkema. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | ISO 179 |
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||
Charpy Impact Unnotched | 2.30 - 7.00 J/cm² | 10.9 - 33.3 ft-lb/in² | Average value: 4.54 J/cm² Grade Count:41 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 2.30 J/cm² | 10.9 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr.. |
|||
Charpy Impact Unnotched | 2.30 - 7.00 J/cm² | 10.9 - 33.3 ft-lb/in² | Average value: 4.49 J/cm² Grade Count:27 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |