Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179 |
PolyOne OnForce™ LFT AM-30LCF/001 Grey Polyphthalamide (PPA) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature -40.0 °C |
22.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature -40.0 °C |
22.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 HS-GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature -40.0 °C |
22.8 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 W-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179 |
PolyOne Bergamid™ B70 G30 grey VN7445CF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179 |
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66 Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1-7004 Polyamide 66, with glass fiber and carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 6-8438-1 Polyamide 12, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105/CF/15 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | IS0179 |
Zhejiang Juner 201-G30 30% Glass Fibre Reinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | IS0179 |
Zhejiang Juner 301-G30 30% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWUVCP 25% Mineral and 15% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide PF003U PA6, 15% Glass Fiber Filled, Injection Molded Staramide PF003U is an 15% Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin, UV Stabilized (also known as Staramide 6 15V S4)Information provided by Eurostar. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179/1eU |
BASF Ultradur B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET Ultradur B 4040 G6 High Speed BK15029 is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179/1eU |
BASF Ultradur B 4406 G4 PBT Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 4.80 J/cm² @Temperature -30.0 °C |
22.8 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® HFD4412 PC (Europe-Africa-Middle East) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Charpy Impact Unnotched | 4.80 J/cm² | 22.8 ft-lb/in² | ISO 179 |
BASF Nypel® 2367G HS BK 15/25% Glass/Mineral Filled PA6 (Dry) Nypel 2367G HS BK-4 is a black pigmented, heat stabilized, 40% mineral and glass fiber reinforced injection molding compound based on recycled PA6 feedstocks. It possesses a balance of engineering .. |