Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.30 - 1.50 J/cm² | 6.19 - 7.14 ft-lb/in² | ISO 11542-2 |
Okulen® 1000 - REG PE Colored OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Charpy Impact Unnotched | 1.30 - 8.00 J/cm² @Temperature -40.0 - -30.0 °C |
6.19 - 38.1 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.15 J/cm² Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit RECONYL A KV30 Recycled nylon 6.6 for injection molding, 30% glass ball reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.30 J/cm² - NB | 6.19 ft-lb/in² - NB | Average value: 5.12 J/cm² Grade Count:16 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact Unnotched | 1.30 J/cm² - NB | 6.19 ft-lb/in² - NB | Average value: 7.57 J/cm² Grade Count:51 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Charpy Impact Unnotched | 1.30 J/cm² - NB @Temperature -40.0 - 30.0 °C |
6.19 ft-lb/in² - NB @Temperature -40.0 - 86.0 °F |
Average value: 5.41 J/cm² Grade Count:27 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Charpy Impact Unnotched | 1.30 - 999.9 J/cm² @Temperature -40.0 - 30.0 °C |
6.19 - 4759 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 3.55 J/cm² Grade Count:49 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 1.30 J/cm² - NB | 6.19 ft-lb/in² - NB | Average value: 8.32 J/cm² Grade Count:79 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact Unnotched | 1.30 J/cm² | 6.19 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 20-8244 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Charpy Impact Unnotched | 1.30 J/cm² | 6.19 ft-lb/in² | ISO 179/1eU |
Polyplastics TOPAS® 5013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) This grade is characterized by its high flowability and superior optical properties. It is suitable for optical components such as lenses and light guide panels where high molded precision is indisp.. |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high .. |
|||
Charpy Impact Unnotched | 1.30 J/cm² | 6.19 ft-lb/in² | EN ISO 179/1eU |
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |
|||
Charpy Impact Unnotched | 1.30 - 1.50 J/cm² | 6.19 - 7.14 ft-lb/in² | ISO 179 |
Vyncolit 2950 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade Injection moldingsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1101 R Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® T20H S63 Polypropylene Car heater casings.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.30 - 1.70 J/cm² | 6.19 - 8.09 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1148 RC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1148 UC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |