Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Okulen® 1000 - REG PE Colored

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Okulen
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Okulen® 1000 - REG PE Colored.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal for applications like machine construction, plant construction, and conveyor technology.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ISO 1183-A
Water Absorption <= 0.10 %
<= 0.10 %
Mechanical Properties Metric English Comments
Hardness, Shore D 63

@Thickness 5.00 mm
63

@Thickness 0.197 in
3 s value; plate; ISO 868
Tensile Strength, Yield 15.0 - 20.0 MPa
2180 - 2900 psi
50 mm/min; ISO/R 527
Elongation at Break >= 50 %
>= 50 %
50 mm/min; ISO/R 527
Creep Strength 10.0 MPa

@Temperature 20.0 °C,
Time 605000 sec
1450 psi

@Temperature 68.0 °F,
Time 168 hour
Charpy Impact Unnotched 1.30 - 1.50 J/cm²
6.19 - 7.14 ft-lb/in²
ISO 11542-2
Coefficient of Friction, Dynamic 0.20

@Pressure 2.00 MPa
0.20

@Pressure 290 psi
PE-metal, V = 10 m/min; ASTM D1894
Abrasion 120 - 140
120 - 140
Slurry-Test rel to GUR 4120 = 100%; DIN 58836
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C
111 µin/in-°F
DIN 53752
Melting Point 133 - 135 °C
271 - 275 °F
DSC ISO 3146
Maximum Service Temperature, Air 80.0 °C
176 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+14 ohm-cm
<= 1.00e+14 ohm-cm
Teil 30; IEC 600093 / VDE 0303
Surface Resistance <= 1.00e+13 ohm
<= 1.00e+13 ohm
Teil 30; IEC 60093 / VDE 0303