Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.30 - 1.60 J/cm² | 6.19 - 7.61 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Charpy Impact Unnotched | 1.40 - 1.60 J/cm² @Temperature 23.0 °C |
6.66 - 7.61 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Charpy Impact Unnotched | 1.20 - 1.60 J/cm² @Temperature 23.0 °C |
5.71 - 7.61 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eU |
Raschig Group EPOXIDUR® 3582 EP Epoxy Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi.. |