Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.40 - 1.70 J/cm² | 6.66 - 8.09 ft-lb/in² | ISO 11542-2 |
Okulen® 1000 PE-UHMW, UV - stabilized OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Thickness 102 mm, Temperature 23.0 °C |
6.66 ft-lb/in² @Thickness 4.00 in, Temperature 73.4 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound PRE-ELEC® PP 1396 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Charpy Impact Unnotched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL A63 CV-CM 0830 9005/Z Powder-coatable nylon 6.6 for injection molding, 8% carbon fiber reinforced, 30% ceramic filled Powder-coatable nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Nilit FRIANYL A63 CV-CM 0830 9005/Z Powder-coatable nylon 6.6 for injection molding, 8% carbon fiber reinforced, 30% ceramic filled Powder-coatable nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Temperature -40.0 °C |
6.66 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 H-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.40 - 1.60 J/cm² @Temperature 23.0 °C |
6.66 - 7.61 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Charpy Impact Unnotched | >= 1.40 J/cm² | >= 6.66 ft-lb/in² | ISO 179 |
Perstorp Compounds AMITEC VXO UF/MF blend A special Urea Formaldehyde/Melamine Formaldehyde blend that enhances surface properties and is optimized for cost-effective injection molding of visible components.Information provided by Perstorp .. |
|||
Charpy Impact Unnotched | 1.40 - 8.00 J/cm² @Temperature -40.0 - 30.0 °C |
6.66 - 38.1 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 5.20 J/cm² Grade Count:84 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Charpy Impact Unnotched | 1.40 - 9.00 J/cm² @Temperature -30.0 - -30.0 °C |
6.66 - 42.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 6.55 J/cm² Grade Count:8 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact Unnotched | 1.40 J/cm² - NB | 6.66 ft-lb/in² - NB | Average value: 12.5 J/cm² Grade Count:21 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Nilit FRIANYL A63 AV15 Nylon 6.6 for injection molding Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.40 - 4.50 J/cm² | 6.66 - 21.4 ft-lb/in² | Average value: 3.24 J/cm² Grade Count:7 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 1.40 - 2.00 J/cm² @Temperature -40.0 - -20.0 °C |
6.66 - 9.52 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.85 J/cm² Grade Count:4 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Charpy Impact Unnotched | 1.40 - 999.9 J/cm² @Temperature -40.0 - 30.0 °C |
6.66 - 4759 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 8.05 J/cm² Grade Count:68 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Charpy Impact Unnotched | 1.40 J/cm² | 6.66 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1301-7767 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo.. |
|||
Charpy Impact Unnotched | 1.40 J/cm² | 6.66 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics ULTEM 3452 PEI (Europe-Africa-Middle East) 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. Resin is RoHS compliant. UL94 V0 and 5VA listing in recognized colors. |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics ULTEM 3452 PEI (Europe-Africa-Middle East) 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. Resin is RoHS compliant. UL94 V0 and 5VA listing in recognized colors. |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Topas Advanced Polymers TOPAS® 6013M-07 Cyclic Olefin Copolymer (COC) TOPAS® 6013M-07 is an injection molding grade with a wide processing window, especially suited for blow molding processes including IBM and ISBM. It is a glass-clear amorphous polymer with outstand.. |
|||
Charpy Impact Unnotched | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 179/IeU |
Addiplast Addilene H 520 M40 Polypropylene Homopolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1040 N Polypropylene Nucleated grade for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1148 TC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.40 J/cm² | 6.66 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7918 PEEK, unreinforced Applications: medical engineeringEspecially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical resistance parts, non flammable.Inherent flame resistance.S.. |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® 348 Q Crystal Clear Transparent 77850 SAN Description: Highly transparent grade with low natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® 348 Q Transparent SAN Description: Highly transparent grade with light natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 1.40 J/cm² - NB | 6.66 ft-lb/in² - NB | Average value: 4.92 J/cm² Grade Count:143 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Charpy Impact Unnotched | 1.40 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
6.66 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.32 J/cm² Grade Count:113 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Charpy Impact Unnotched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LARTON K/30 30% Carbon Fiber Reinforced Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Charpy Impact Unnotched | 1.40 - 1000 J/cm² | 6.66 - 4760 ft-lb/in² | Average value: 1.40 J/cm² Grade Count:8 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact Unnotched | 1.40 J/cm² | 6.66 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has .. |