Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL PD G523 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-25-20 High impact injection moulding grade. Other characteristics: good flow, excellent thermal stabilit.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | |
Ineos ABS Lustran® H604 Standard impact strength.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | |
Ineos ABS Lustran® H701 Medium heat resistance, high impact strength. ,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature 23.0 °C |
85.7 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Forsan® 483 Acrylonitrile Butadiene Styrene (ABS) High heat resistant, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Kau.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® C 50 H2 PA6, DRY Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 BKB086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 18.0 J/cm² | 85.7 ft-lb/in² | |
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultraform H 4320 Q600 POM Ultraform H4320 Q600 is an extrusion POM high molecular weight grade. This grade enables high extrusion rates with thick-walled product. It also exhibits high thermal stability and a low tendency .. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultraform N 2310P Q600 POM Ultraform N2310P Q600 is a general-purpose injection molding POM grade containing special lubricant. Low frictional coefficient giving extremely low wear with otherwise unaltered mechanical propert.. |
|||
Charpy Impact Unnotched | 18.0 J/cm² @Temperature -30.0 °C |
85.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |