Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 H-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced
Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 W-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 CU90 Nylon 6.6 for injection molding, 90% copper filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.90 J/cm²

@Temperature -40.0 °C
9.04 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 BR80 Nylon 6.6 for injection molding, 80% bronze filled
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.90 J/cm²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LATISTAT 30/R-05 High Impact Strength Polystyrene Base Conductive Plastic  (discontinued **)
Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable..
Charpy Impact Unnotched 1.90 J/cm²

@Temperature -30.0 °C
9.04 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Nilit FRIANYL A63 KV25 Nylon 6.6 for injection molding, 25% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 20-7796 Polyphthalamide, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1301-0915 PPS, linear, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Charpy Impact Unnotched 1.90 J/cm²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® 378 P Crystal Clear Transparent SAN
Description: Easy-flow grade with enhanced resistance to chemicals.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
Styrolution NOVODUR® P2HGV ABS, 16% Glass Fiber
Injection molding grade, glass reinforced (16%).Applications: Automotive industry: instrument panels, rear light housings, internal components of domestic appliances.
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
Notched/Unnotched not specified; ASTM DIN53453
Total PPC 4624WZ Polypropylene, Impact Copolymer
ATOFINA 4624WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4624WZ is characterized by significantly improved resistance, while maintaining exce..
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
ISO 179/IeU
Addiplast Addilene H 242 M40 Polypropylene Homopolymer
High heat resistance, detergent stabilizedInformation provided by Addiplast.
Charpy Impact Unnotched 1.90 J/cm²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
Charpy Impact Unnotched 1.90 J/cm²

@Temperature -30.0 °C
9.04 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Appryl® CZT 1030 Polypropylene, 30% Talc/Mica Filled
Compound of a PP copolymer modified with EPR and 30% of a mixture of talc and mica. This grade has been specially developed for exterior automotive applications, that required an excellent thermal d..
Charpy Impact Unnotched 1.90 J/cm² - NB
9.04 ft-lb/in² - NB
Average value: 4.44 J/cm² Grade Count:32
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Charpy Impact Unnotched 1.90 - 2.00 J/cm²
9.04 - 9.52 ft-lb/in²
Average value: 1.97 J/cm² Grade Count:3
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
Arkema Group Oroglas® VM Acrylic, Injection Molding Grade  (discontinued **)
OROGLAS VM is an injection molding grade with a medium heat resistance and easy flow.OROGLAS VM is particularly suitable to improve mold filling of technical parts.The VM L version has been speciall..
Charpy Impact Unnotched 1.90 J/cm²
9.04 ft-lb/in²
Arkema Group Oroglas® VS-UVT Acrylic, Injection Molding Grade  (discontinued **)
The outstanding flow of OROGLAS VS-UVT makes it as the material of choice for injection molding of part with thin wall thickness.The ultraviolet transmitting ( uvt) formulation is developed to meet ..
Charpy Impact Unnotched 1.90 - 3.50 J/cm²
9.04 - 16.7 ft-lb/in²
Average value: 2.54 J/cm² Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Charpy Impact Unnotched 1.90 - 5.00 J/cm²

@Temperature -30.0 - 30.0 °C
9.04 - 23.8 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 3.19 J/cm² Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved