Polymer Property : Izod Impact, Unnotched = 0.420 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.420 J/cm
0.787 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON EV008 PEI
LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural.
Izod Impact, Unnotched 0.420 - 1.00 J/cm
0.787 - 1.87 ft-lb/in
Notch Status Unknown
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal
High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head..
Izod Impact, Unnotched 0.420 - 1.00 J/cm
0.787 - 1.87 ft-lb/in
Notch Status Unknown
Goodfellow Evanohm® Precision Resistance Nickel Alloy
Electrical resistance alloy with a very low temperature coefficient of resistivityInformation provided by Goodfellow.