Polymer Property : Izod Impact, Unnotched = 1.97 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.97 J/cm
3.69 ft-lb/in
ASTM D412
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Izod Impact, Unnotched 1.97 J/cm
3.69 ft-lb/in
ASTM D412
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Izod Impact, Unnotched 1.97 J/cm
3.69 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP UX06425 PPA
LNP* LUBRICOMP* UX06425 is a compound based on Polyphthalamide (PPA) containing 10% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Hot Water Moldable and Heat Stab..
Izod Impact, Unnotched 1.97 J/cm

@Temperature 23.0 °C
3.69 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC
LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by..
Izod Impact, Unnotched 1.97 J/cm

@Temperature 23.0 °C
3.69 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific)
LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b..
Izod Impact, Unnotched 1.97 J/cm
3.69 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP WX05456 Polyester, TP
LNP THERMOCOMP* WX05456 is a compound based on Polyester, TP resin containing Mineral.