Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D412 |
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Izod Impact, Unnotched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D412 |
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Izod Impact, Unnotched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UX06425 PPA LNP* LUBRICOMP* UX06425 is a compound based on Polyphthalamide (PPA) containing 10% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Hot Water Moldable and Heat Stab.. |
|||
Izod Impact, Unnotched | 1.97 J/cm @Temperature 23.0 °C |
3.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by.. |
|||
Izod Impact, Unnotched | 1.97 J/cm @Temperature 23.0 °C |
3.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific) LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b.. |
|||
Izod Impact, Unnotched | 1.97 J/cm | 3.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WX05456 Polyester, TP LNP THERMOCOMP* WX05456 is a compound based on Polyester, TP resin containing Mineral. |